Inconel 601 Barra Brionnaithe Fuar Tarraingthe
Comhdhéanamh Ceimiceach As Inconel 601 Barra Babhta
|
Grád |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
|
Inconel 601 |
0.10 uas |
1.00 uas |
0.50 uas |
0.015uas |
1.00 uas |
Iarmhéid |
58.0 – 63.0 |
21.0 – 25.0 |
Inconel 601 Barraí Geala Airíonna Meicniúla
|
Grád |
C |
Mn |
Si |
S |
Cu |
Fe |
Ni |
Cr |
|
Inconel 601 |
0.10 uas |
1.00 uas |
0.50 uas |
0.015uas |
1.00 uas |
Iarmhéid |
58.0 – 63.0 |
21.0 – 25.0 |
Inconel 601 Barra Brionnaithe Airíonna Fisiceacha
|
Eilimint |
Dlús |
Leáphointe |
Neart Teanntachta |
Neart Táirgeachta (0.2% Fritháireamh) |
Fadú |
|
Inconel 601 |
8.1 g/cm3 |
1411 céim (2571 céim F) |
Psi – 80,000 , MPa – 550 |
Psi – 30,000 , MPa – 205 |
30 % |
Gráid Choibhéiseacha Barra Babhta Inconel 601 Fuar Tarraingthe
|
CAIGHDEÁN |
OIBREACHA NR. |
UNS |
JIS |
BS |
GOST |
AFNOR |
GA |
|
Inconel 601 |
2.4851 |
N06601 |
NCF 601 |
NA 49 |
XH60BT |
NC23FeA |
NiCr23Fe |