Inconel 718 Bar Bhabhta Cóimhiotail

Maidir le barra bhabhta cóimhiotail 718 inconel 718
Inconel 718 Is nicil {- cóimhiotal cróimiam é barra bhabhta cóimhiotail - a bhfuil aithne air as a neart ard, a fhriotaíocht creimthe, agus a tháthú den scoth, go háirithe ag teochtaí arda. Is deascadh é {- cóimhiotal cruaite, rud a chiallaíonn gur féidir a neart a mhéadú go suntasach trí chóireáil teasa. Fágann sé seo go bhfuil sé oiriúnach do raon leathan feidhmchlár, lena n -áirítear aeraspáis, ola agus gás, agus próiseáil cheimiceach.
Cad é comhdhéanamh an bharra bhabhta Inconel 718?
Is é atá i gceist le Inconel 718 Round Bar ná nicil - Barra cóimhiotail cróimiam le cion nicil suas le 55%. Tá cróimiam 17% ann freisin, 4.9% niobium, agus iarann 6.6% ar a laghad, chomh maith le alúmanam, bórón, carbón, cóbalt, copar, mangainéis, fosfar, luaidhe, sulfair, agus sileacain.

Comhdhéanamh Ceimiceach Cóimhiotail 718 slata
| Grád | Ni | Cc | Rise | C | MN | S | Meandar | SI | Tosaigh |
| Inconel 718 | 50 – 55 | 17 – 21 | 0.3 uasmhéid | 0.08 max | 0.35 uasmhéid | 0.015 max | 2.8 – 3.3 | 0.35 uasmhéid | 1.0 Max |
Airíonna Meicniúla Inconel 718 barraí
| Dlús | Leáphointe | Neart teanntachta | Neart táirgeachta (0.2%fritháirithe) | Élagáil |
| 8.2 g/cm3 | 1350 céim (2460 céim F) | PSI - 135,000, MPA - 930 | PSI - 70,000, MPA - 482 | 45 % |
Cruas an chóimhiotail inconel 718 barra bhabhta
| Strus cruthúnas 0.2% | Neart teanntachta | Édáileáil | Laghdú ar an Limistéar | Cré |
|---|---|---|---|---|
| MPA | MPA | % | % | HAD |
| Mí Miannach | Mí Miannach | Mí Miannach | Mí Miannach | Mí Miannach |
| 827 | 1034 | 17 | 25 | 40 |
Cairt méide de bharra nicil 718
| Méid & Toisí Inconel 718 Barra Babhta | |||||||
|---|---|---|---|---|---|---|---|
| Meicniúil | Barra na Stát Aontaithe | Astm/ Ceanada | Seapánach | ||||
| Méid an bharra | Diam. (mm) | Méid an bharra | Diam. (Orlach) | Méid an bharra | Diam. (MM2) | Méid an bharra | Diam. (mm) |
| 5 | 5 | #2 | 0.250 | 10M | 100 | 6 | 6 |
| 5.5 | 5.5 | #3 | 0.375 | 15M | 200 | 10 | 10 |
| 6 | 6 | #4 | 0.500 | 20M | 300 | 13 | 13 |
| 7 | 7 | #5 | 0.718 | 25M | 500 | 16 | 16 |
| 8 | 8 | #6 | 0.750 | 30M | 700 | 19 | 19 |
| 9 | 9 | #7 | 0.875 | 35M | 1000 | 22 | 22 |
| 10 | 10 | #8 | 1.000 | 45M | 1500 | 25 | 25 |
| 11 | 11 | #9 | 1.125 | 55M | 2500 | 29 | 29 |
| 12 | 12 | #10 | 1.250 | 32 | 32 | ||
| 14 | 14 | #11 | 1.375 | 35 | 35 | ||
| 16 | 16 | #12 | 1.500 | 38 | 38 | ||
| 18 | 18 | #13 | 1.718 | 41 | 41 | ||
| 20 | 20 | #14 | 1.750 | 44 | 44 | ||
| 22 | 22 | #15 | 1.875 | 48 | 48 | ||
| 25 | 25 | #16 | 2.000 | 51 | 51 | ||
| 28 | 28 | #18 | 2.250 | 57 | 57 | ||

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, agus cóimhiotail ardteochta. Úsáidtear táirgí Gnee Steel go forleathan in iarratais aeraspáis, ceimiceacha, leictrigh, feithicleach agus fuinnimh núicléiche. Cuirimid réitigh chóimhiotail saincheaptha ar fáil freisin atá saincheaptha do riachtanais na gcustaiméirí. Maidir le fiosrúcháin phraghsála cóimhiotail nó réitigh chóimhiotail saincheaptha, déan teagmháil linn le haghaidh luachana agss@gneesteel.com.