Pláta cóimhiotail Monel 400
Cruach Gnee
Maidir le pláta cóimhiotail Monel 400
Is nicil {- Pláta Alloy Monel 400 - a bhfuil aithne air as a fhriotaíocht creimthe den scoth, go háirithe i dtimpeallachtaí mara agus ceimiceacha, chomh maith lena neart ard agus inmharthanacht mhaith. Is ábhar ildánach é a úsáidtear in iarratais éagsúla, lena n -áirítear druileáil ola amach ón gcósta, próiseáil cheimiceach, agus innealtóireacht mhuirí.

Cruach Gnee
Cad chuige a n -úsáidtear pláta cóimhiotail Monel 400?
Úsáidtear pláta Monel 400 go forleathan sna tionscail cheimiceacha, peitriliam agus mara. Tairgeann sé friotaíocht creimthe i dtimpeallachtaí éagsúla mara agus ceimiceacha, ó uisce íon go neamh - aigéid mhianracha, salainn, agus alcaileacha a ocsaídiú.

400 Comhdhéanamh pláta tarraingthe fuar snasta monel
| Grád | C | MN | SI | S | Rise | Fe | Ni |
|---|---|---|---|---|---|---|---|
| Monel 400 | 0.30 uasmhéid | 2.00 Max | 0.50 uasmhéid | 0.024 Max | 28.00 – 34.00 | 2.50 Max | 63.00 nóiméad |
400 Pláta Alloy Saintréithe Meicniúla
| Eilimint | Dlús | Leáphointe | Neart teanntachta | Neart táirgeachta (0.2%fritháirithe) | Élagáil |
|---|---|---|---|---|---|
| Monel 400 | 8.8 g/cm3 | 1350 céim (2460 céim F) | PSI - 80,000, MPA - 550 | PSI - 35,000, MPA - 240 | 40 % |
Airíonna Teirmeacha Pláta 400 Pláta Monel
| Teocht | Leathnú meánach líneach | Seoltacht theirmeach | Teas sonrach | Friotachas leictreach | |||||
| Céim F | céim | i/ in/ céim f x 10-6 | µm/m • Céim | Btu - i/h/ft | W/m • Céim | BTU/ LB/ Céim F | J/kg • Céim | ohm - ciorcal mil/ft | µΩ•m |
| -320 | -200 | - | - | - | - | - | - | 205 | 360 |
| -300 | -180 | 6.1 | 11.1 | 113 | 16.5 | 0.05 | 223 | - | - |
| -200 | -130 | 6.4 | 11.4 | 130 | 18.2 | 0.078 | 320 | - | - |
| -100 | -70 | -6.7 | 12.1 | 139 | 19.8 | 0.088 | 378 | - | - |
| 70 | 21 | - | - | 151 | 22 | 0.102 | 427 | 307 | 0.511 |
| 200 | 100 | 7.7 | 14.2 | 167 | 24 | 0.105 | 445 | 332 | 0.537 |
| 400 | 200 | 8.6 | 15.2 | 193 | 26.9 | 0.11 | 459 | 337 | 0.559 |
| 600 | 300 | 8.8 | 15.7 | 215 | 30.1 | 0.114 | 470 | 346 | 0.574 |
| 800 | 400 | 8.9 | 16.1 | 238 | 33.4 | - | - | 355 | 0.587 |
| 1000 | 500 | 9.1 | 16.3 | 238 | 36.5 | - | - | 367 | 0.603 |
| 1200 | 600 | 9.3 | 16.6 | 287 | 39.4 | - | - | 379 | 0.62 |
| 1400 | 700 | 9.6 | 17 | 311 | 42.4 | - | - | 391 | 0.639 |
| 1600 | 800 | 9.8 | 17.4 | 335d | 45.5d | - | - | 403 | 0.658 |
| 1800 | 900 | 10.0d | 17.7 | 360d | 48.8d | - | - | 415 | 0.675 |
| 2000 | 1000 | 10.3d | 18.1d | - | - | - | - | 427 | 0.692 |

Gnee Steel is a company specializing in the production of various nickel-based alloys, nickel 201, nickel202, hastelloy c-276, hastelloy c-22, hastelloy b, hastelloy c-4, Inconel alloy 600, Inconel 625, Inconel 718, Inconel x-750, incoloy alloy 800, incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500 agus ábhair chóimhiotail ardteochta. Déanann sé speisialtóireacht i dtáirgeadh agus díolachán ábhar cóimhiotail. Úsáidtear táirgí Gnee Steel go forleathan in aeraspáis, i gcumhacht cheimiceach, i gcumhacht leictreach, i ngluaisteán, i bhfuinneamh núicléach agus i réimsí eile, agus is féidir leo réitigh ábhar cóimhiotail saincheaptha a sholáthar de réir riachtanais na gcustaiméirí. Má theastaíonn uait a bheith ar an eolas faoin gcomhairliúchán ar phraghsanna ábhar cóimhiotail nó má sholáthraíonn tú réitigh ábhar cóimhiotail saincheaptha, tá fáilte romhat teagmháil a dhéanamh linn ag am ar bith chun luachan a fháil agss@gneesteel.com