Incoloy 800
This nickel-iron-chromium alloy has good strength and excellent resistance to oxidation and carburization in high temperature environments. Incoloy 800 is also corrosion resistant in many aqueous environments and has been used in some steam power plants due to its resistance to stress cracking.

What is INCOLOY 800 heating element?What is INCOLOY 800 heating element?

Incoloy 800 is also known as Nicrofer 3220, Nicrimphy 800 and Pyromet 800.


Incoloy 800 has the following key features:




Incoloy 800 is suitable for the following applications:





W.NR 1.4876
UNS N08800
AWS 020

The chemical composition of Incoloy 800 is indicated in the table below:

30.00 35.00
– 2.00
– 0.75
19.00 23.00
0.15 0.60
C – 0.10
– 1.00
– 1.50
0.15 0.60
S – 0.015